EN 10210 Structrual Tube
Delivery time: 15-45 days (based on quantity) after receiving advanced payment by T/T or LC .
Part 1 of this European Standard describes in detail the technical conditions of delivery of hot-worked hollow sections of round, square and rectangular cross-section, but also the technical conditions of delivery of heat-treated or non-heat-treated hot-worked hollow sections immediately after heat treatment, as well as the technical conditions of delivery of cold-worked hollow sections heat-treated in order to obtain properties like those of hot-worked products. Fine-grained structural steels are in principle delivered in the normalized condition.
These requirements apply to ordinary and high-quality non-alloyed structural steels, as defined in EN 10020, as well as to fine-grained non-alloyed high-quality steels and alloyed special steels.
The grades, chemical compositions and mechanical properties of ordinary and high-quality structural steels are listed in Appendix A.
Fine grain non-alloy steel and alloy special steel grades, chemical composition and mechanical properties are listed in Appendix B.
The products specified in this European Standard are suitable for use in steel structures. Dimensions and deviations and hydrostatic values are listed in Part 2 of this standard (EN102102).

EN10210 Carbon Steel Welded Pipe Specification
| En 10210 S420nh S420nlh S460nh S460nlh Structural Square Steel Tube | |
| Square pipe: 20*20mm~500*500mm Rectangular pipe: 20*40mm~300*500mm Thickness: 1.2mm~20mm Length: 2.0m~12m |
|
| Q195=S195 / A53 Grade A Q235=S235 / A53 Grade B / A500 Grade A / STK400 / SS400 / ST42.2 Q355=S355JR / A500 Grade B Grade C |
|
| EN10219, EN10210 GB/T 6728 JIS G3466 ASTM A500, A36 |
|
| ISO 9001,CE | |
| 1. OD 300mm and below In hexagonal seaworthy bundles packed by steel strips, With two nylon slings for each bundles 2. above OD 300mm in bulk or according to custom opinion 3. 25 tons/container and 5 tons/size for a trial order; 4. For 20" container the max length is 5.8m; 5. For 40" container the max length is 11.8m. |
|
| 15-45 days (based on quantity) after receiving advanced payment by T/T or LC . | |
A: Yes, we are a manufacturer, not an agent. We are a manufacturer with 16 years experience in producing steel pipes and fittings. We have our own factories in Shandong, Tianjin and Henan, China. You can get the real factory price and quality from us. Welcome to contact us!
A: All products are subject to three inspections during the whole manufacturing process, such as production, cutting, packaging, etc. The factory inspection report is provided with the shipment, and third-party inspections, such as SGS, can be accepted if required.
Populárne Tagy: en 10210 structrual tube, China en 10210 structrual tube manufacturers, suppliers, ERW oceľové potrubie, Jis G3445 Elektrické zvárané potrubie, Jis G3466 uhlíkové oceľové štvorcové trubice, Odpor zvárané potrubie, Round SA135 rúrky, S235jr
Tiež sa vám môže páčiť
Zaslať požiadavku